Preparation and characterization of silk fibroin as a biomaterial with potential for drug delivery
Preparation and characterization of silk fibroin as a biomaterial with potential for drug delivery
Blog Article
Abstract
Background
Degummed silk fibroin from
Methods
In this study, we treated degummed silk with four kinds of calcium-alcohol solutions, and performed secondary structure measurements and enzyme activity test to distinguish the differences between the regenerated fibroins and degummed silk fibroin.
Results
Gel electrophoresis analysis revealed that Ca(NO3)2-methanol, Ca(NO3)2-ethanol, or CaCl2-methanol treatments produced more lower molecular weights of silk fibroin than CaCl2-ethanol.X-ray diffraction and Fourier-transform infrared spectroscopy showed that CaCl2-ethanol produced a crystalline structure with more silk I (α-form, type II β-turn), while the other treatments produced more silk II (β-form, anti-parallel β-pleated sheet).
Solid-State 13C cross polarization and magic angle spinning-nuclear magnetic resonance measurements suggested 6 that regenerated fibroins from CaCl2-ethanol were nearly identical to degummed silk fibroin, while the other treatments produced fibroins with significantly different chemical shifts.Finally, enzyme activity test indicated that silk fibroins from CaCl2-ethanol had higher activity when linked to a known chemotherapeutic drug, L-asparaginase, than the fibroins from other treatments.
Conclusions
Collectively, these results suggest that the CaCl2-ethanol processing method produces silk fibroin with biomaterial properties that are appropriate for drug delivery.